PU STAR is a benzene-free and ketone-free polyurethane gravure surface printing ink suitable for various treatments of polyolefin films, featuring excellent environmental friendliness and printability.
Detailed
PU STAR is a benzene-free and ketone-free polyurethane gravure surface printing ink suitable for various treatments of polyolefin films, featuring excellent environmental friendliness and printability.
Product uses and features
1.It is suitable for processing OPP, CPP, PET, PE, etc.
2.The printed materials have very little residual solvent and excellent environmental protection performance.
3.The color is bright and the gloss is good.
4.It has strong adhesion and good resistance to rubbing and scratches.
5.It has good printing adaptability and can adapt to printing at different machine speeds.
Reference color
The base colors include 110 White, 280 Yellow, 360 red, 800 blue, 1000 Black, 330 golden red, 235 yellow, 170 red, 471 Peony, 515 orange, 518 orange, 300 orange, 500 purple, 930 green, 001 ink oil, etc. Special color samples can be prepared according to the user's requirements.
Dilution and printing viscosity
|
white ink solvent: |
2-N-BUTOXYETHYL METHACRYLATE/ Isopropyl alcohol=80/20 |
|
color ink solvent: |
N-propyl ester/Propanol/1-Methoxy-2-propanol=85/10/5 |
|
※If slow drying is required, N-propyl ester or Butyl ester can be used to replace some esters |
|
white ink: 13~15 s, color ink: 14~16 s ※ 3#Charn Cup
The ratio of printing viscosity and thinner can be adjusted accordingly according to the printing pattern, drying capacity, printing speed and printing effect.
Instructions for the Use of Curing agent
PUSTAR series inkIt can be used for two-component purposes to enhance the performance of the ink. Curing agent addition: TCS-4394 addition amount: 1-3%
Performance improvement: Increase composite strength, temperature resistance, adhesion, etc
Disposal of old ink: Leftover ink with added curing agent should not be stored for a long time. When using it again, mix it with new ink (old ink <30%) and add the curing agent again. Pay attention to reverse adhesion.
Notes
1.If there are requirements for heat resistance and higher anti-adhesion, 2% to 4% TCS-4394 curing agent must be added for use and cured at 50℃ for more than 48 hours.
2.The surface treatment requirement for the printing substrate is ≥38 dynes. If the substrate is weakly treated for printing, it needs to be confirmed by yourself before use. For printing on films other than the above-mentioned ones or on special films, please contact our company.
Environmental protection regulations
1Complies with the requirements of regulations such as GB4806.14, GB4806.1, and GB31603;
2.Comply with the requirements of regulations such as ROHs, REACH, and EN71-3;
3.Comply with the standard QB/T 1046 "Gravure Plastic Film Composite Ink". 4. This product complies with the NL rules formulated by the Japan Printing Ink Association.
Product application cases
|
Packaging classification |
Specific examples |
|
Hygienic packaging |
Diapers, sanitary napkins, tissues, masks, etc |
|
Food packaging |
Sandwiches, enoki mushrooms, snack packaging, etc |